A complete guide to making high-resolution screen prints with minimal tools.
Notes: When applying film emulsion to the screen, the matte surface should face the screen. The glossy surface is the plastic backing, which is removed later, just before exposure.
The resolution test shown in the video actually indicates line width, not pitch. So, the 1mm sample has 1mm lines and 1mm spaces. Thus, the pitch is actually 2mm.
The Nazdar paint instructions say there is a 30 minute "induction" period that is needed for the catalyst to start working. Nope. Just weigh out the paint and catalyst, mix, and immediately apply to the screen. Print the needed items quickly, and clean it off the screen as soon as possible. Use disposable mixing cups / tools. It is *messy*!
Shopping list:
Pre-stretched screen: https://www.mclogan.com/shop/aluminum-12x17-p-1173-c-293_297_379_3.html
Squeegee: https://www.mclogan.com/shop/squeegees-per-inch-durometer-p-5-c-293_297_1_4.html
Epoxy paint: https://www.mclogan.com/shop/nazdar-ade-series-epoxy-screen-ink-p-1145.html
Paint cleaner: https://www.mclogan.com/shop/mclogan-graphic-press-wash-p-156.html
Emulsion remover: https://www.mclogan.com/shop/mclogan-emulsion-remover-concentrate-p-149-c-187_42_44.html
Degreaser: https://www.atlasscreensupply.com/store/p/163-ICC-858-Stain-Remover/Degreaser-Quart.aspx
Film emulsion: https://www.atlasscreensupply.com/store/p/772-DuraCap-11-x-14.aspx
Vellum paper: https://www.amazon.com/Office-Depot-Premium-Translucent-Vellum/dp/B014SBHGMQ/
Consider using 365nm LEDs instead of fluorescent tubes for exposure.
https://www.patreon.com/AppliedScience
Random question, can multiple pressure washers be as strong as an industrial waterjet cutter?
ReplyDeleteHi Ben, your project begs the question about reproducing small, custom LCD displays for hand-held testers. Possible to duplicate or totally impractical? Basically, I would be starting with the content of the display with layout, but no ‘electrical’ connections to the segments. Thanks Ben, Doug
ReplyDelete