It looks like it might be possible to glue delrin with 3M DP-8005 after this chromic acid etching process. I'll do some more testing later.
I mixed:
40g water
25g potassium dichromate
500g concentrated sulfuric acid
http://books.google.com/books?id=Fl57...
I guess this mixture is commonly called chromic acid.
Things that I should have done:
Use a Pyrex beaker
Don't use the magnetic stirrer, just use a teflon stir stick
Use an ice bath at the beginning of the procedure